- +8613394156633
- +8618753175317
- +8613364256389
- carolyn.shi@resterchem.com
- 18753175317,13364256389,18842852758
Mining, ship 90℃ Ethylene propylene insulated rubber Insulating rubber material implement the standards of MT818 mining coal cable, obey the regulation of XJ-30A in the GB7594.8-87.the product also meet the…
Mining, ship 90℃ Ethylene propylene insulated rubber
Insulating rubber material implement the standards of MT818 mining coal cable, obey the regulation of XJ-30A in the GB7594.8-87.the product also meet the rules of ship cable insulated material EPR in the IEC60092-351:2004.
This series of product mainly falls into the catalogue, YHJ-30A (8.7/10kV or below ), YHJ-30Z (3.6/6kV or below), YHJ-30D (0.66/1.14kV or below ) etc.
Performance comparison
Test item | Unit | MT818 GB7594.8-87 | YHJ-30A Test value | ||
Before ageing | Tensile strength | Intermediate values | MPa | ≥6.5 | 8.2 |
Elongation at | Intermediate values | % | ≥200 | 330 | |
Heat ageing test of air box | Aging conditions | Temperature | ℃ | 135±2 | |
Time | h | 7×24 | |||
Tensile strength | Intermediate values | MPa | & nbsp; | 9 | |
Rate of change | % | ≤±30 | 10 | ||
Elongation at | Intermediate values | % | & nbsp; | 275 | |
Rate of change | % | ≤±30 | -6 | ||
Air bomb ageing test | Test conditions | Temperature | ℃ | 127±1 | |
Time | h | 40 | |||
Tensile strength | Rate of change | % | ≤±30 | 15 | |
Elongation at | Rate of change | % | ≤±30 | -10 | |
Hot set test | Test conditions | Temperature | ℃ | 250±3 | |
Load time | min | 15 | |||
Mechanical stress | MPa | 0.2 | |||
Load elongation | % | ≤175 | 25 | ||
Permanent deformation after cooling | % | ≤15 | 10 | ||
Ozone resistance test
& nbsp; |
Test conditions | Temperature | ℃ | 25±2 | |
Time | h | 24 | |||
Ozone concentration | % | 0.025~0.030 | |||
Test results | & nbsp; | No cracks | No cracks |